Preparation method of graphite block

Aug 19, 2021

Leave a message

The preparation of graphite blocks is very important. Each product weight must be just right to produce high-quality graphite blocks.

1, 70 to 90 parts of anthracite, 5 to 10 parts of a catalyst element or its compound, and 10 to 20 parts of silica;

2. Crush and mix the components evenly, put them into the press, and increase the temperature and pressure;

3. Raise the temperature to 400℃~1000℃, the pressure is 10~50KPa;

4, heat preservation for 10-40 minutes; this method directly uses coal to produce artificial graphite to produce graphite blocks. The process is simple and easy to implement, the energy-saving benefits are outstanding, the specific gravity of the product is slightly lighter, the particle size is 0.05-1mm, the performance is not inferior, and the lubrication performance is good. 